ASTM A27 Grade 70-36 Cast Steel: Composition, Properties and the 60-30 and 65-35 Grades

ASTM A27 covers carbon steel castings for general applications. In its grade names the first number is the minimum tensile strength and the second the minimum yield strength, both in ksi: 70-36 means 70 ksi (485 MPa) and 36 ksi (250 MPa). This page compares 70-36 with 60-30 and 65-35.

JK Casting · Buyer resource · Updated 16 November 2026

What ASTM A27 70-36 is

ASTM A27/A27M is the US specification for carbon steel castings for general application. Its grades include N-1, N-2, U-60-30, 60-30, 65-35, 70-36 and 70-40. Grade 70-36 [485-250] is the strongest of the three grades compared here, with up to 0.35% carbon. ASTM A216 (WCB) is the separate specification for pressure-containing parts in high-temperature service.

70-36, 65-35 and 60-30 compared

Scroll sideways to see the whole table

ASTM A27/A27M-20, Table 1, maximum values; tensile values are minimums.
GradeC max., %Mn max., %Min. tensile, MPaMin. yield, MPaMin. elongation, %Min. reduction of area, %
70-36 [485-250]0.350.704852502230
65-35 [450-240]0.300.704502402435

Grade 60-30 [415-205] requires 415 MPa tensile and 205 MPa yield, with carbon up to 0.30% and manganese up to 0.60%. All three grades allow up to 0.80% silicon and 0.035% each of sulfur and phosphorus in the 2020 edition; older editions allowed more, so check which edition the drawing cites. For each 0.01% of carbon below the maximum, more manganese is allowed, up to a limit set in the standard.

70-36 compared with WCB and Chinese grades

Scroll sideways to see the whole table

Approximate comparison. The standard on the drawing governs; substitution needs buyer approval.
GradeStandardMin. yield, MPaTensile, MPaMin. elongation, %How it compares
70-36ASTM A27 (USA)250485 min.22Reference grade
WCBASTM A216 (USA)250485–65522Same minimum tensile and yield; A216 also sets a tensile maximum of 655 MPa
ZG270-500GB/T 11352 (China)270500 min.18Higher minimum yield and tensile strength, lower minimum elongation

These equivalents are approximate, not identical materials. Composition limits, test methods and heat treatment differ between standards. The standard named on the drawing governs, and any substitution needs the buyer’s written approval.

Heat treatment and welding

Heat treatment. ASTM A27 requires grades 60-30, 65-35 and 70-36 to be heat treated by annealing, normalising, normalising and tempering, or quenching and tempering.

Welding. The A27 grades are intended to be suitable for fusion welding to other steel castings or wrought steel, but they do not all weld equally well; agree the welding procedure for the part.

How JK Casting makes ASTM A27 castings

JK Casting makes carbon steel castings to customer drawings in Gaomi, Shandong, China. Parts are sand cast, including shell moulding in resin-coated sand, or made by lost-wax investment casting; investment castings made in-house weigh up to about 20 kg each. Castings are supplied raw or machined, and JK machines only the castings it makes. Each drawing is quoted separately, with tooling and unit price on separate lines.

For a quotation, send the drawing with the full grade designation and standard, the heat treatment condition and any tests the part needs. Material records such as EN 10204 3.1 certificates are provided when agreed for the order.

Related pages: Steel castings · Investment casting · Sand casting · What to put on a casting drawing · Send a drawing for quotation

Frequently asked questions

What does ASTM A27 70-36 mean?

70 is the minimum tensile strength and 36 the minimum yield strength, both in ksi. In SI units the grade is written 70-36 [485-250], meaning 485 MPa tensile and 250 MPa yield.

What is the difference between ASTM A27 70-36 and A216 WCB?

Both require at least 485 MPa tensile and 250 MPa yield. A27 is for general application; A216 is for pressure-containing parts in high-temperature service and also sets a tensile maximum of 655 MPa.

Which A27 grade should a drawing name?

The one the design calls for, with its standard, for example “ASTM A27 70-36”. Grades 60-30 and 65-35 have lower strength minimums and higher minimum elongation.

What is the Chinese equivalent of ASTM A27 70-36?

No GB grade is identical. ZG270-500 is often compared with it: 270 MPa yield, 500 MPa tensile and 18% elongation, against 250 MPa, 485 MPa and 22% for 70-36.

Standards referenced: ASTM A27/A27M-20; ASTM A216/A216M-21; GB/T 11352-2009.