Custom castings from your drawings or samples. Send your requirements for a quotation.Request a Quote
Jiangkai Casting logoJK CastingDrawing-based OEM metal parts

Material reference

Cast Stainless Steel Grades: CF8, CF8M, CF3 and CF3M Equivalents

Cast stainless parts are specified as CF8 or CF8M on a US drawing, ZG07Cr19Ni10 on a Chinese one, 1.4408 on a European one. This chart compares the four common austenitic casting grades, their wrought counterparts (304, 304L, 316, 316L) and what to write on an RFQ.

JK Casting · Buyer resource · Updated 16 November 2026

The comparison is approximate

These equivalents are approximate, not identical materials. Composition limits, test methods and heat treatment differ between standards. The standard named on the drawing governs, and any substitution needs the buyer’s written approval.

How to read CF grade names

CF8, CF3, CF8M and CF3M follow the ACI casting designation system. C marks a corrosion-resistant casting grade, the next letter marks the alloy type, the number is the maximum carbon content in hundredths of a percent (8 = 0.08%, 3 = 0.03%), and M marks molybdenum. So CF3M is the low-carbon, molybdenum-bearing grade.

Composition and tensile minimums (ASTM A351)

Scroll sideways to see the whole table

ASTM A351 limits, % by mass; tensile values are minimums.
GradeC max.CrNiMoTensile / yield, MPaElongation, %Wrought counterpart
CF80.0818.0–21.08.0–11.0≤0.50485 / 20535304
CF30.0317.0–21.08.0–12.0≤0.50485 / 20535304L
CF8M0.0818.0–21.09.0–12.02.0–3.0485 / 20530316
CF3M0.0317.0–21.09.0–13.02.0–3.0485 / 20530316L
CF8C0.0818.0–21.09.0–12.0≤0.50485 / 20530347

CF8C is stabilised with niobium (columbium): at least 8 times the carbon content and at most 1.00%. It has a higher minimum solution-annealing temperature in ASTM A351 than the other grades in this table.

ASTM A351 covers austenitic castings for pressure-containing parts; ASTM A743 lists the same grade names for general-service corrosion-resistant castings. Tensile values are minimums from ASTM A351; elongation is measured over 50 mm. In ksi: tensile 70, yield 30.

Chinese, European and Russian equivalents

Scroll sideways to see the whole table

Approximate comparison. The standard on the drawing governs; substitution needs buyer approval.
ASTMGB/T 2100-2017 (China)EN 10213 (Europe)ГОСТ 977-88 (Russia), nearest by composition
CF8ZG07Cr19Ni101.4308 (GX5CrNi19-10)10Х18Н9Л; 12Х18Н9ТЛ (titanium-stabilised)
CF3ZG03Cr19Ni111.4309 (GX2CrNi19-11)No grade with carbon at or below 0.03%
CF8MZG07Cr19Ni11Mo21.4408 (GX5CrNiMo19-11-2)12Х18Н12М3ТЛ (titanium-stabilised, Mo 3.0–4.0%)
CF3MZG03Cr19Ni11Mo21.4409 (GX2CrNiMo19-11-2)No grade with carbon at or below 0.03%

The ГОСТ 977-88 grades are the nearest by published composition, not equivalents: they allow more carbon (up to 0.12–0.14%), and 12Х18Н12М3ТЛ has more molybdenum than CF8M. ГОСТ 977-88 lists no austenitic grade with carbon at or below 0.03%, so CF3 and CF3M have no direct counterpart there.

Cast grades and 304 / 316

CF8 and CF8M are the cast counterparts of wrought 304 and 316, not the same materials. Their composition limits differ from the wrought grades, and a cast austenitic structure normally contains some ferrite. If a drawing for a cast part names 304 or 316, agree the casting grade (for example CF8 or CF8M) in writing before quoting.

Heat treatment and welding

Heat treatment. ASTM A351 requires these grades to be solution annealed at 1040 °C (1900 °F) minimum, then quenched in water or rapidly cooled by other means. Weld repairs are made with procedures and welders qualified to ASTM A488.

The low-carbon grades CF3 and CF3M are chosen when parts are welded and corrosion resistance next to the weld matters, because low carbon reduces carbide precipitation in the heat-affected zone.

How JK Casting supplies stainless steel castings

JK Casting reviews every stainless steel casting part by part. Send the drawing, the grade with its standard and any corrosion or test requirements, and JK confirms the casting route, investment casting or sand casting, before quoting. Investment castings made in-house weigh up to about 20 kg each. Castings are supplied raw or machined, and JK machines only the castings it makes. Each drawing is quoted separately, with tooling and unit price on separate lines.

Related pages: Cast stainless steel grades chart · Investment casting · Steel castings · What to put on a casting drawing · Send a drawing for quotation

Frequently asked questions

What is the difference between CF8 and CF8M?

CF8M contains 2.0–3.0% molybdenum and CF8 at most 0.50%; CF8M also has a slightly higher nickel range. Molybdenum improves resistance to pitting, so CF8M is the cast counterpart of 316 and CF8 of 304.

What does the 3 in CF3 and CF3M mean?

It is the maximum carbon content in hundredths of a percent: 0.03% for CF3 and CF3M, against 0.08% for CF8 and CF8M. The low-carbon grades are the cast counterparts of 304L and 316L.

What is the Chinese equivalent of CF8M?

The nearest GB/T 2100-2017 grade is ZG07Cr19Ni11Mo2. The equivalents are approximate, so the drawing’s standard governs and a substitution needs approval.

Is CF8 the same as 304?

No. CF8 is the cast counterpart of wrought 304. Its composition limits differ, for example chromium 18.0–21.0% in ASTM A351, and the cast structure normally contains some ferrite.

Standards referenced: ASTM A351/A351M; ASTM A743/A743M; GB/T 2100-2017; EN 10213; ГОСТ 977-88.